Notice: Function _load_textdomain_just_in_time was called incorrectly. Translation loading for the wordpress-seo domain was triggered too early. This is usually an indicator for some code in the plugin or theme running too early. Translations should be loaded at the init action or later. Please see Debugging in WordPress for more information. (This message was added in version 6.7.0.) in /var/www/html/wp-includes/functions.php on line 6260 Detangling Conditioner - Happi
Hair Care

Detangling Conditioner

Detangling Conditioner
Ingredients
%

Phase A

  • Deionized water
  • 61.60

0

  • Dissolvine 220-S (Coast Southwest, Akzo Nobel Functional Chemicals LLC) (Tetrasodium EDTA)
  • .10
  • Endinol SCS (Coast Southwest) (Sodium coco-sulfate)
  • 2.00
  • Allantoin (Coast Southwest, 3V Inc.) (Allantoin)
  • .20
  • TEA 99% (Coast Southwest) (Triethanolamine)
  • 3.40
  • DL-Panthenol, 75% (Coast Southwest) (DL Panthenol)
  • 2.00
  • Endimate 33V (Coast Southwest) (Caprylic/capric triglyceride)
  • 8.00
  • Refined olive oil (Coast Southwest) (Olea Europaea (olive) fruit oil)
  • 2.00
  • Stearic acid (Coast Southwest)
  • 5.00
  • Palmitic acid (Coast Southwest)
  • 1.00
  • Conditioner P10 (Coast Southwest, 3V Inc.) (Polyquaterium 10)
  • 1.00
  • Xylitol
  • .10
  • Abiol (Coast Southwest, 3V Inc.) (Imidazolidinyl urea)
  • .50
  • Polysorbate 20 (Coast Southwest) (Polysorbate 20)
  • 1.00
  • Fragrance
  • .20

Phase B

  • Cetyl stearyl alcohol (Coast Southwest)
  • 2.00

Phase C

  • Deionized water
  • 6.40

Phase D

  • Deionized water
  • 3.00

Phase E

  • Phenoxyethanol (Coast Southwest) (Phenoxyethanol)
  • .50

Procedure

Fill main vessel with phase A. Begin mixing and heat to 70-75°C. In side vessel, add phase B and heat to 70-75°C. When phase A and phase B are at temperature and homogeneous, slowly add phase B to phase A with mixing and homogenizing. Begin cooling slowly with mixing. At 45-50°C, add premixed phase C to combined phase A and B. Premix phase D and add, followed by premixed phase E. Switch to slow speed and transfer to holding vessel. Allow batch to thicken for 24 hours and take pH and viscosity.

Properties

pHu20146.4 (24 hrs.); Viscosityu2014Spindle #4 at 2.5 rpm u2013 124,000 cps

More Information

Coast Southwest, Inc.
800-621-0500
Email: info@coastsouthwest.com
Website: www.coastsouthwest.com